http://repositorio.unb.br/handle/10482/30457
Arquivo | Tamanho | Formato | |
---|---|---|---|
ARTIGO_ IntemperismoArtificialLaminas.pdf | 1,09 MB | Adobe PDF | Visualizar/Abrir |
Título: | Intemperismo artificial em lâminas de Tectona grandis tratadas com produtos de acabamento |
Autor(es): | Queiroz, Francis Lívio Corrêa Gonçalez, Joaquim Carlos Del Menezzi, Cláudio Henrique Ribeiro, Edilene Silva Lima, Clarissa Melo |
Assunto: | Árvores Fotodegradação Colorimetria |
Data de publicação: | Out-2016 |
Editora: | Instituto de Florestas da Universidade Federal Rural do Rio de Janeiro |
Referência: | QUEIROZ, Francis Lívio Corrêa et al. Intemperismo Artificial em lâminas de Tectona grandis tratadas com produtos de acabamento. Floresta e Ambiente, Seropédica, v. 23, n. 4, p. 573-581, out./dez. 2016. Disponível em: <http://www.scielo.br/scielo.php?script=sci_arttext&pid=S2179-80872016000400573&lng=en&nrm=iso>. Acesso em: 12 dez. 2017. Epub Mar 22, 2016. doi: http://dx.doi.org/10.1590/2179-8087.126315. |
Resumo: | Este estudo teve por objetivo avaliar a ação do tempo de exposição ao intemperismo artificial na cor de lâminas de madeiras de teca tratadas com produtos de acabamento. Amostras que receberam 2 tipos de produto, a seladora e o stain, mais as testemunhas, sem acabamento. O experimento foi instalado no delineamento inteiramente casualizado, com 3 tratamentos e 4 repetições. As lâminas ficaram expostas ao simulador QUV-Acelerated Weathering Teste, por 7 períodos, de: 6, 12, 24, 48, 96, 192 e 384 horas. Após cada período de intemperismo foram feitas medições das cores, com espectrofotômetro COLOR EYe XTH. As variáveis cromáticas avaliadas foram: L*, a*, b*, C e h*. Ao final do estudo pôde-se concluir que as lâminas de madeira de teca sofreram alterações em sua cor com o passar do tempo de exposição e que o stain apresentou maior eficiência na conservação da cor da madeira. |
Abstract: | This study aims to evaluate the effects of weather exposure to artificial weathering in the color of teak wood veneer treated with finishing products. The samples received 2 types of products, the sealer and the stain, plus witnesses, unfinished. The experiment was conducted in a completely randomized design with 3 treatments and 4 replications. Slides were exposed to QUV-Accelerated Weathering Test simulator for 7 periods as follow: 6, 12, 24, 48, 96, 192 and 384 hours. Color measurements were made after each period of weathering using the spectrophotometer Color Eye XTH. The chromatic variables evaluated were: L *, a *, b *, C * and h*. The study concluded that the teak wood veneer had color alterations with the exposure time and the stain was more efficient in preserving the wood color. |
Licença: | Floresta e Ambiente - Este é um artigo publicado em acesso aberto (Open Access) sob a licença Creative Commons Attribution, que permite uso, distribuição e reprodução em qualquer meio, sem restrições desde que o trabalho original seja corretamente citado (CC BY 4.0). Fonte: http://www.scielo.br/scielo.php?script=sci_arttext&pid=S2179-80872016000400573&lng=en&nrm=iso. Acesso em: 12 dez. 2017. |
DOI: | http://dx.doi.org/10.1590/2179-8087.126315 |
Aparece nas coleções: | Artigos publicados em periódicos e afins |
Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.